3003 vs 3004 Aluminum Coil for Roll Forming
When comparing 3003 vs 3004 aluminum coil for a roll-formed profile, start with the feature that determines whether the part passes inspection. For a tight return hem that cracks at the fold, trial 3003 in a temper suited to the bend. For a channel that stays bent after the load comes off, evaluate 3004 at the specified thickness. If the channel springs back fully but flexes too much in use, review the section dimensions and support span first.
3003 vs 3004 Aluminum Coil: What Does the Profile Need to Do?
Mark the critical feature on the cross-section drawing. Agree with the roll former on when to measure it: at cutoff, under load, or after the load is removed. Each check answers a different purchasing question.
| Profile requirement | Starting point for the inquiry | Trial observation that matters |
|---|---|---|
| Tight return on a trim strip | Ask for 3003 in a condition suitable for the intended bend | Inspect the outside of the return and check the closed gap on a cut length |
| Channel stays bent after the load is removed | Ask whether a suitable 3004 temper can meet the material and forming requirements | Measure the free section, then check permanent set after the agreed load is removed |
| The channel flexes too far under load but returns to shape | Review section depth, sheet thickness, span and supports with the designer before changing alloy | Measure deflection at the specified load and span, then verify recovery after unloading |
What the alloy and temper tell you
Both alloys belong to the aluminum-manganese family. Magnesium in 3004 helps it develop higher strength than 3003 under comparable conditions. Temper describes the condition of the metal as delivered. In these alloys, rolling and subsequent processing affect strength and the amount of further deformation the strip can tolerate. An alloy number on its own gives the mill too little information to reproduce the behavior of an approved coil.
Suppose one mill quotes 3003-H14 and another quotes 3004-H24. H14 means the metal reached its temper through strain hardening. H24 means it was strain hardened and then partially annealed. The final digit 4 denotes nominal half-hard temper in each case. It does not specify one yield strength or one allowable bend radius for both coils.
To compare the alloys, ask both mills to quote the same nominal thickness and a comparable temper, and to identify the property limits in the applicable product standard. If the available offers are H14 and H24, mark each trial coil with its full alloy and temper. A successful hem or load test then qualifies that particular combination for engineering review.
Use the 3003 aluminum coil specifications to frame the first option. Voyage Metal also lists 3004 in its aluminum coil range. For the second option, specify the same gauge and slit width, and ask which temper the supplier can offer. Give the supplier the section drawing before treating any catalog description as an offer against your specification.
Separate material strength from profile stiffness
Suppose a cover channel deflects too much between its supports. Identify whether it springs back to its original shape when unloaded or retains a bend. Those observations lead to different engineering questions. Changing to a higher-strength alloy may help address permanent deformation. Elastic deflection also depends heavily on the section geometry, thickness, span and support conditions. The designer should review those inputs before procurement changes the alloy.
For the trial, agree on where and how the section will be supported, the load to apply, and the dimensions to record during loading and after unloading. A sample described simply as “stiffer” gives the next shift little to reproduce. A marked drawing and the two measurements let the buyer compare trial runs without relying on how each sample feels in the hand.
Specify the strip your line can accept
Start with nominal thickness and its permitted variation. Give slit width its own tolerance. A purchase order stating only the finished outside width of the channel leaves the supplier guessing which developed strip width the roll former has approved. If that width is still being established, label it as a trial value and state who will release the production value after the trial.
A slit edge can end up at the visible return or under a concealed overlap. Mark the edge that matters and state any burr restriction and inspection method required by the drawing. If the strip wanders at the entrance guides, discuss camber as well. Camber is the sideways curve along the length of the strip. An agreed reference length makes a camber measurement meaningful to both parties.
Confirm the coil inside diameter against the uncoiler mandrel. Ask for the maximum outside diameter and individual coil weight the line and handling equipment can take. Specify winding direction when an exposed face must feed a particular way. Two suppliers may quote the same total tonnage in quite different coil sizes. Ask for the proposed weight per coil and the number of coils per delivery. A lower price per tonne may come with more line stops to thread new coils.
Run a trial that purchasing can repeat
Choose a profile that includes the difficult feature, such as the tightest return or the longest unsupported leg. Keep the drawing revision, strip width, measured incoming thickness and material lot with the sample. Record the major line settings and any correction needed to reach the target shape. If the operator adjusts a stand for the second coil, retain that information with the result. It may be essential when the order returns to the line months later.
Inspect the profile in its specified condition after cutoff. Where fit matters, use a mating part or an agreed gauge. Where appearance matters, agree on which face is visible, when any protective film comes off and how the surface will be examined. If a supplier proposes a new alloy or temper for an existing part, obtain drawing-owner approval before converting the trial into a production order.
Make the trial decision easy to carry back to purchasing. For example, record whether the return closed cleanly, whether the cut ends fit the gauge, and which coil identification appears on the accepted sample. Write down who approved the result. When the mill later proposes a different temper or slit tolerance, the buyer can see which checks to repeat before releasing it.

FAQ
Can I switch from 3003 to 3004 and reduce the thickness?
Treat thinner gauge as a design change. The change affects bend geometry, section stiffness and possibly fit with the mating part. Ask the designer which load, dimensional and service requirements must be demonstrated. Trial the proposed gauge and condition against those requirements and record the approved revision before releasing a purchase order.
What if our old purchase order gives the alloy but no temper?
Look for the material certificate and receiving record of a coil that ran successfully. Match the lot number to a retained part or production record if available. If the condition still cannot be traced, have suppliers identify their proposed temper explicitly and agree on a trial. That creates a reference for the next purchase.
What to include in a coil RFQ
Copy this line into your inquiry and attach the profile drawing. If you want both alloys quoted, ask for separate offers against the same drawing revision and have each supplier flag any deviation.
Drawing / revision: ___
Application: ___
Alloy and temper options: ___
Thickness × slit width, with tolerances: ___
Coil ID / maximum OD / maximum coil weight: ___
Quantity / destination: ___
Include the governing standard, finish, edge condition, inspection documents and packing instructions where specified. Send your coil requirements to Voyage Metal for a material and quotation review.